can anyone give advise as to wether this layup will provide enough strength on my 20 ft to support the power of a 225hp engine
original outer skin left intact
a layer of probond by fgi used to stick ply to skin
2 x 18mm struct marine ply bonded together with layer of 300gm cs mat
all clamped to outer skin till cured
all joins coved
4 x layers of 600gm cs matt
2 to 3 extra layers of 600gm cs matt at the edges for tabbing
and thats it
do i need to add more mat or will this be ok?